  • (4) Poly Etch Rate Variation
  • Wider spacing between Poly fingers ? faster etch
    rate.

2
  • Multi strip Poly resistors ? strips on the ends
    need Dummy strips

3
  • Closed-loop Dummies ? problem due
    to inductive interaction with EM fileds.
  • Either break them up (fig.7.7) or at least have a
    gap to stop current path.
  • Dummies need electrical contact to the Tank.

4
  • (5) Diffusion interactions
  • Consider diffused-base resistors (fig.7.8)
  • Diffused resistors usually are laid in a Tank
    with NBL.
  • Edges of diffused areas have diffusion tails. ?
    resistors occupying the ends slightly
    different values. ? use dummy resistors
    (fig.7.8)

5
  • Layouts designs for serpentine resistors
    (fig.7.9)
  • Layouts in Tanks with deep-N sinkers (fig.7.9)

6
  • (6) Stress Gradients and Package Shifts
  • Packaging can exert stress onto Die.
  • Metal Can package, Ceramic package, and Plastic
    package

Metal Can package
7
Ceramic package, and Plastic package
8
  • Metal Can package or Ceramic package ? lowest
    stress
  • Use metal header plate, mounted using Epoxy.
  • Solder or gold eutectic mounting ? higher stress
  • Plastic package ? higher stress
  • Epoxy resin for mounting
  • Residual stress due to difference in CTE of Si
    and Epoxy
  • Shifts in Offset voltage in OpAmp, Comparators,
    or output ref. Voltage ? Package shifts

9
Coefficients of Thermal Expansion (CTE)
10
  • Piezoresistivity
  • N-type (100) Si
  • Maximum piezoresistivity along lt100gt
  • Minimum along lt110gt gtN-type diffused resistors
    along lt110gt

11
  • P-type (100) Si
  • Maximum along lt110gt
  • Minimum along lt100gt
  • P-type diffused resistors along lt100gt

12
  • (111) Si ? isotropic

13
  • Gradients and Centroids
  • Stress distribution on a Die surface isobaric
    contour plot

14
  • Place matched devices at Regions of lowest
    stress gradients.

15
  • Place matched devices at Regions of lowest
    stress gradients.

16
  • Matched devices must reside as close as possible
    ? minimize the stress
    difference
  • Centroid of the device center of stress
    distribution

17
  • Common-Centroid Layout
  • Example
  • Two matched devices, A and B.
  • Each device consists of two sections.

18
  • Segmenting devices
  • 1. Finding the greatest common factor
  • Example 10kW and 25 kW ? 5kW segment size
  • 2.Use the smaller device as basic segment
    remainder should be gt 70
  • Example 39.7kW and 144.3 kW ?
  • Case-1 Use 39.7kW as a single segment. ?
    144.3/39.7 3.637 (3 segments 25.2kW 64)
  • Case-2 Divide 39.7kW into two segments ?
    unit 39.7 19.85kW ? 39,7kW 2 segments
    144.3 144.3/7.27 7 segments
    27 of unit.
  • Case-3 Divide 39.7kW into 3 segments ? unit
    39.7/3 13.233kW ? 39.7kW 3 segments
    144.3kW 144.3/13.233 10.904 10 segments
    90 (11.97kW).
  • 3.Do not use too small a segment.
  • 4.Make partial R segment using a sliding contact.
  • 5.Capacitor segments should not have dimensions
    much less than 100 mm2.

19
  • Coincidence, Symmetry, Dispersion, and
    Compactness

1-dimensional
20
  • Coincidence, Symmetry, Dispersion, and
    Compactness

2-Dimensional
  • Cross-coupled pair

21
  • Coincidence, Symmetry, Dispersion, and
    Compactness

2-Dimensional
  • Cross-coupled pair
  • Tiling

22
  • (7) Temperature and Thermoelectric Effect
  • DIP or SOIC Tj Ta Pd qja
  • Tj Junction temperature
  • Ta ambient temperature
  • Pd power dissipated in package
  • qja junction-to-ambient thermal impedance
  • 16-pin DIP qja 110 C/W
  • 16-pin surface-mount (SOIC) qja 131 C/W
  • Power package Tj Tc Pdqjc
  • Tc case temperature
  • qja junction-to-case thermal impedance.
  • 3-lead plastic TO-220 Power Package qja 4.2
    C/W
  • 3-lead metal TO-3 can power package qja 2.7

23
  • Thermoelectric effect ET S DTc
  • S Seeback coefficient ( 0.4mV/C)
  • DTc temperature difference between two contacts
    of the resistor
  • Example 0.4mV offset in Bipolar mirror produces
    1.5 mismatch in the currents.

Power device
24