Ink as a Substrate - PowerPoint PPT Presentation

About This Presentation
Title:

Ink as a Substrate

Description:

Polyamide Ink Base - Effect of Primer A Coat Weight. Bond. Bond. Bond. Bond. Bond. Bond. 83.00 38.00 44.00 50.00 71.00 32.00 . Title: PowerPoint Presentation Author ... – PowerPoint PPT presentation

Number of Views:90
Avg rating:3.0/5.0
Slides: 21
Provided by: War102
Learn more at: https://www.iopp.org
Category:

less

Transcript and Presenter's Notes

Title: Ink as a Substrate


1
Ink as a Substrate in Flexible Packaging
Laminations

Presented by Bruce Foster Mica Corporation
IOPP Technical Bag Committee Winter 2013 Meeting
2
Better Understand Effects of
  • Ink Type (polymer base)
  • Ink Color

Objective
On Adhesion in Extrusion Laminations
(with PRIMERS, of course!)
3
12-micron polyester film 1-side factory treated
  • Inks solvent-based, toluene-free
  • 3 chemistries
  • Vinyl-modified polyurethane
  • Modified-polyamide
  • Modified-polyurethane

Materials
4
12-micron polyester film 1-side factory treated
Inks 3 chemistries
  • Primers Water-Based
  • 2 chemistries
  • Polyethylene-imine
  • Polyurethane

Materials
5
Lab Experiments Set I
  • Ink draw-downs on polyester film
  • Different types colors
  • Prime over printed samples
  • Polyethylene-imine based extrusion primer

Approach
  • Extrusion-coat on lab pilot line
  • High-temperature polyethylene

6
Lab Experiments Set I
40-micron polyethylene _at_ high temperature
Approach
primer
ink
12-micron polyester film (corona-treated)
7
Ink lift-off
12-micron polyester film (corona-treated)
8
All Samples - Ink lift-off
9
Ink Splits
Ink lift-off
10
Lab Experiments Set I
  • Modified Polyamide Inks had best adhesion to
    polyester film
  • Polyethylene-imine primer works with all inks
    tested

Learnings
3. White inks had lowest adhesion to films
11
???
12
(No Transcript)
13
Lab Experiments Set II
  • Pre-prime polyester film
  • Both imine and urethane primers
  • Print over primed samples
  • Vinyl-modified polyurethane inks

Approach
  • 3. Prime over printed samples
  • Both imine and urethane primers
  • 4. Extrusion-coat on lab pilot line
  • High-temperature polyethylene

14
Lab Experiments Set II
40-micron polyethylene _at_ high temperature
Approach
primer
Vinyl-modified polyurethane inks
primer
12-micron polyester film (corona-treated)
15
Results Set IIa
Pre-Primer InkColor Post-Primer Bonds,g/25mm Failure Mode
Imine White Imine gt500 Inseparable
Imine Blue Imine 400 Film Tear
Imine White on blue Imine 93 Ink lift-off
Imine White Urethane 400 Film Tear
Imine Blue Urethane gt500 Inseparable
Imine White on blue Urethane gt500 Inseparable
Results
16
Results Set IIb
Pre-Primer InkColor Post-Primer Bonds,g/25mm Failure Mode
Urethane White Imine 200 Ink lift-off
Urethane Blue Imine gt500 Inseparable
Urethane White on blue Imine gt500 Inseparable
Urethane White Urethane 170 Ink lift-off
Urethane Blue Urethane gt500 Inseparable
Urethane White on blue Urethane gt500 Inseparable
Results
17
Lab Experiments Set II
  • Pre-priming works for vinyl-modifed polyurethane
    inks!
  • Both primer chemistries gave mostly good results

Learnings
3. Polyethylene-imine pre-primer was best for
white ink adhesion
18
Lab Experiments Set I
  • Modified Polyamide Inks had best adhesion to
    polyester film

Learnings
  • Polyethylene-imine primer works with all inks
    tested

3. White inks had lowest adhesion to films
19
P.T. Colorpak Indonesia, Tbk.
Jonida Gjika Lab Chemist
Mica Corporation
Thanks
TAPPI PLACE
20
Thanks, for your attention!
Questions?
Bruce Fosterbfoster_at_mica-corp.com
Write a Comment
User Comments (0)
About PowerShow.com